Skip to main content

Table 1 Analysis results of Ca and P concentrations on the surfaces of Ti–6Al–4V ELI alloy plate specimens of the UT, AH, and APH groups immersed in SBF for 1 day

From: Improvement of osseointegration of Ti–6Al–4V ELI alloy orthodontic mini-screws through anodization, cyclic pre-calcification, and heat treatments

 

UT

AH

APH

Ca (wt%)

0.06

27.34

P (wt%)

12.45

Ca/P (at%)

1.70